Oxidation Resistance Superalloy Inconel Pipe 0.299 lbs / in3 8.28 g / cm3 980℃

Oxidation Resistance Superalloy Inconel Pipe 0.299 lbs / in3 8.28 g / cm3 980℃

Brand Name : Torich
Model Number : Inconel X-750
Certification : CE PED
Place of Origin : China
MOQ : 1000kg
Price : 6000-20000 USD per ton
Payment Terms : L/C, T/T
Supply Ability : 200 tons per year
Delivery Time : 6-8 weeks
Packaging Details : In bundles in wooden box
Contact Now

Inconel Steel Tue are produced with Inconel Alloy Steel Grade InconelX-750


Mechanical component

C:≤0.08

Cr:14.0-17.0

Ni+Co:≥70.0

Al:0.40-1.00

Ti:2.25-2.75

Fe:5.00-9.00

Nb+Ta:0.70-1.20

Co:1.00max

Mn:1.00max

Si:0.50max

S:0.010max

Cu:0.50max

P:0.015max


Data for material physical properties:


Desity : 0.299lbs/in3,8.28g/cm3


InconelX-750 thermal conductivity

θ/℃50100300500900

λ/(W/(m·℃))

14.715.920.125.137.3

InconelX-750 line expansion coefficient

θ/℃20~20020~30020~40020~50020~60020~70020~800
α/10-6℃-113.113.514.114.415.015.616.2

Characteristic:

InconelX-750 alloy Nickel-base superalloy.


Below 980℃ with good resistance ro corrosion and oxidation resistance

Below 800℃ has higher strength

Below 540℃ has good resistance to relaxation properties, good formability and weldability as well.


Application is aircraft engines.


Heat treatment process:

Annealing 955-1010℃,water-cooled

Weldment before welding annealing 980℃,1h

weldement stress relief annealing900℃ moisture 2h

Stress relief annealing 885℃,±15℃,24h,air cooling.


InconelX-750 mechanical properties.


σb/MPa≤965

σP0.2/MPa≤550

δ4D/%≥35


with the condition of 980 ℃ ± 15 ℃, holding the appropriate time, air cooling or rapid cooling, descaling.


σb/MPa≥1170

σP0.2/MPa≥790

δ4D/%≥15


with the condition of+ 730 ℃ ± 10 ℃, 8h, furnace cooling 55 ℃ / h or air cooling to 620 ℃ ± 10 ℃, 8h, air-cooled, the total aging time is not less than 18h


Related standard:AMS 5542,AMS 5598


Application for engine part.



Product Tags:

Stainless Steel Seamless Tube

      

Welded Stainless Steel Tube

      
China Customized Inflatable Bumper Ball Game Bubble Adult Grass CE supplier

Oxidation Resistance Superalloy Inconel Pipe 0.299 lbs / in3 8.28 g / cm3 980℃ Images

Inquiry Cart 0
Send your message to this supplier
 
From:
To: TORICH INTERNATIONAL CO.,LTD
Subject:
Message:
Characters Remaining: (0/3000)
 
Inquiry Cart 0